Kappa SS creep testing machine

Kappa SS

The Kappa SS creep-testing machine is equipped with a central lead-screw and is suitable for creep tests and advanced creep tests requiring maximum precision in force control.

  • load frame with single lead-screw drive and precision guidance provided via 4 steel columns, giving precise axial loading and maximum durability
  • load string with optimum alignment properties in accordance with ASTM E 292
  • high-resolution force and travel measurement for optimum control properties, especially at very low test speeds
  • constant moving crosshead speed via precision central ball-screw
  • optional digital closed-loop force and strain control
  • creep tests and stress relaxation tests; user-programmed load-cycles
  • large range of machine accessories for flexible application options, complemented by intelligent electronics and software